Submitted by tr_admin on Tue, 06/11/2013 - 10:49
Forums:
To achieve the max. performance, the recommended working distance is 5mm.
The tip of the Quatz rod should not be touching to your sample, as it would react with your sample material and the rod can get cloudy by the reaction.
The other working distance can be used but there would be compromise to the temperature achievement.